ESKOBROWN

ESKOBROWN Images

ESKOBROWN

ESKOBROWN Description

ORIGIN FINLAND
BLOCK SIZES ALLDIMENSIONS
COLOUR UNIFORMITY EXCELLENT
AVAILABILITY EXCELLENT
PREVAILING USE INTERIORANDEXTERIOR
POLISHING TREATMENT EXCELLENT
OTHER SURFACE TREATMENTS EXCELLENT
GENERAL COMMENTS

ONE OF THE MOST USED MATERIAL ALL AROUND THE WORLD. WHEN POLISHED, A PRIOR SELECTION IS RECOMMENDED, ALSO SHOWS VERY SMALL CHINKS LIKE A NET. CONTROL ABOUT GRAIN DIRECTION IS REQUIRED.
EXAMPLES OF TEST RESULTS:

COMPRESSIVE STRENGTH 1980Kg./cm.. 2010Kg./cm..
DITTO AFTER GELIVITY 1625Kg./cm.. 1628Kg./cm..
WATER ABSORPTION 0,25% 0,28%
ULTIMATE TENSIL STRENGTH 128Kg./cm.. 132Kg./cm..
IMPACT TEST-MIN. FALL HEIGHT 62cm. 65cm.
THERMAL COEFF. EXPANSION 0,0068mm./m.C 0,0065mm./m.C
ABRASION COEFFICIENT
BULK DENSITY 2745Kg./m.. 2749Kg./m..
ELASTICITY MODULE 554000Kg./cm.. 557000Kg./cm..
KNOOP MICROHARDNESS
FLEXURAL STRENGTH
POROSITY